Cross-grade comparison

Film Selection Guide

Every value below is copied from the published datasheet on that grade's own product page — nothing here is estimated. Where a cell reads “—”, the figure has not been measured or released yet, and you should ask us rather than assume.

Which film grade do I need for my forming depth?

Sorted shallowest to deepest. Forming depth is the single most common starting point for a thermoforming enquiry — find your depth, then check the barrier and sterilization tables for the same grade.

Forming depth by grade — values from each grade's published datasheet.
GradeStructureThicknessForming depthTypical use
F4538MPP / PE co-extrusion80 μm10–15 mmVacuum thermoforming base film for medical device packaging
F2624Nylon / PE (NL)80 μm10–15 mmSealing film for continuous automatic vacuum thermoforming
F2624-MNylon / PE (NE)80 μm10–15 mmVacuum thermoforming base film for medical device packaging
15N01NY(PA) / EVOH / PE139 μm10–30 mm
F2615Nylon / PE (NL)120 μm10–30 mmFood vacuum thermoforming packaging
F2615-MNylon / PE (NE)120 μm10–30 mmDeep-draw vacuum thermoforming base film for sterilized medical equipment
F2703Nylon / PE (NE)110 μm10–30 mmVacuum thermoforming base film for medical device packaging
F1127NY(PA) / EVOH / PE80 μm15 mm
F4539MPP / PE co-extrusion120 μm30 mmDeeper-draw vacuum thermoforming base film for medical device packaging
F2235Nylon / Retort CPP (NY/RCPP)135 μm30–50 mmVacuum packaging film for room temperature, refrigerated, and frozen food; sous-vide
F2237Nylon / Retort CPP (NY/RCPP)150 μm30–50 mmVacuum packaging film for room temperature, refrigerated, and frozen food; sous-vide
F2606-MNylon / PE (NE)150 μm30–50 mmDeepest-draw vacuum thermoforming base film for large sterilized medical equipment
153B2PPNY/RCPP133 μm30–50mm
F1154NY(PA) / EVOH / PE150 μm40–50 mm
F2606Nylon / PE (NL)150 μm40–50 mmSealing/forming film for continuous automatic vacuum thermoforming, deep-draw
F2647Nylon / PE (NL)180 μm60–70 mmSealing/forming film for continuous automatic vacuum thermoforming, extra-deep draw
15309Nylon / PE (NL)262 μm60–100 mmDeep-draw sealing film for continuous automatic vacuum thermoforming

Which grades survive retort, and what sterilization do they accept?

Retort grades are grouped by product line. “E.O.” is ethylene oxide; gamma is r-ray irradiation. Medical grades list sterilization compatibility rather than a temperature rating.

Heat resistance and sterilization compatibility by grade.
GradeProduct lineThicknessHeat resistanceSterilization
F4531Easy Peel Film30 μm121–130°C
F4568Easy Peel Film35 μm130°C
F4569Easy Peel Film50 μm130°C
F45A5Easy Peel Film50 μm130°C
F45A7Easy Peel Film70 μm130°C
F4538Nylon & MPP/PE Film — Medical Care Package80 μmE.O. (ethylene oxide) sterilization
F2624-MNylon & MPP/PE Film — Medical Care Package80 μmE.O. and gamma (r-ray) sterilization
F2703Nylon & MPP/PE Film — Medical Care Package110 μmE.O. and gamma (r-ray) sterilization
F4539Nylon & MPP/PE Film — Medical Care Package120 μmE.O. (ethylene oxide) sterilization
F2615-MNylon & MPP/PE Film — Medical Care Package120 μmE.O. and gamma (r-ray) sterilization
F2606-MNylon & MPP/PE Film — Medical Care Package150 μmE.O. and gamma (r-ray) sterilization
F2235Nylon / Retort CPP Thermoforming Film135 μm
F2237Nylon / Retort CPP Thermoforming Film150 μm
F4513Retort CPP Film70 μm130°C
153B2Retort CPP Film133 μm121°C retort sterilization

How do Intlpak’s EVOH structures compare on oxygen barrier?

Lower OTR means a better oxygen barrier. All values are measured at 20°C / 65% RH. Structure determines both barrier level and which sealing process the film suits.

EVOH oxygen transmission rate by structure, best barrier first.
GradeStructureThicknessOTR (cc/m²·24hr)Forming depth
F1154NY(PA) / EVOH / PE150 μm0.31 cc/m²·24hr40–50 mm
15N01NY(PA) / EVOH / PE139 μm0.5 cc/m²·24hr10–30 mm
F1256PE / EVOH / PE60 μm0.65 cc/m²·24hr
F1127NY(PA) / EVOH / PE80 μm0.8 cc/m²·24hr15 mm
F1201PE / EVOH / PE45 μm0.9 cc/m²·24hr
F1257PE / EVOH / PE55 μm1.3 cc/m²·24hr
F1648-EPLPP / EVOH / PE45 μm1.3 cc/m²·24hr
F1645PP / EVOH / PE45 μm1.3 cc/m²·24hr
F1249PE / EVOH / PE40 μm2.6 cc/m²·24hr
F1302PP / EVOH / PP40 μm2.6 cc/m²·24hr
F1307PP / EVOH / PP70 μm2.6 cc/m²·24hr
F1355PP / EVOH / PP55 μm2.6 cc/m²·24hr

How to read this page. Values are representative or measured figures from official datasheets, not guaranteed minimums — confirm against your own line trial. A dash means Intlpak has not published that figure for that grade; we will not substitute a number from a neighbouring grade.

Not sure which grade fits your line?

Send us your forming depth, shelf-life target and sterilization method — we will shortlist the grades that qualify and arrange samples.